Part Number Ordering Information, example and explanation:
CDR01BX100AKSR where,
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
|
Part number ordering options are developed using the following criteria:
Tolerance |
Finish |
|
||
|
S = Solder-coated, final | M = 1.0%/1000 hrs (Level 3) | ||
|
M = Palladium-Silver | P = 0.1%/1000 hrs (Level 2) | ||
|
N = Silver-Nickel-Gold | R = 0.01%/1000 hrs (Level 2) | ||
|
U = Base Metallization-Barrier, Metal-Solder Coated | S = 0.001%/1000 hrs (Level 1) | ||
|
W =
Base Metallization-Barrier, Metal-Tinned (Tin or Tin/Lead Alloy)
(PROHIBITED FOR SPACE FLIGHT USE. SEE APPLICATION NOTE) |
|||
|
Y = Base Metallization Barrier 100% Tin (PROHIBITED FOR SPACE FLIGHT USE. SEE APPLICATION NOTE) | |||
|
||||
|